The most possible extreme powerful professional flash powder KClO4 Al S 50/40/10 potassium perchlorate aluminum sulfur.

It was originally developed for coarser homemade aluminum where 70/30 KClO4/Al burned slow. And with more KClO4, or more Sulfur the composition was slow too.

For small firecrakers i use 3-7 micron dark aluminum powder.

For large firecrackers i use 50:50 mixture 3-7 micron Dark+30 micron aluminum powder mixture to get a large effect. Or cc 20 micron around ball milled aluminum. Similar are a Ba(NO3)2/KClO4/Al/S 30/30/30/10 mixture with the same mixed Al, but there you must use 2% boric acid. The Dark+Mixed Al 50:50 mixture operates under 40 micron aluminum.

More:

The most possible extreme powerful professional flash powder

Whats the most powerful professional flash powder what you can make at home,safe,extreme bright,the voice is sharp, and the destruction power was amazing too.About 10 year research i find the perfect flash powder. I tested all possible flash powders with all possible of ratio this time. And nothing can beat it.This flash powder was the KClO4/Al/S 50/40/10% (Potassium perchlorate/Aluminium/Sulfur) with 3-4 micron german dark aluminum powder.

If you make firecrackers this flash powder was the best what you can make it at home. There are no disadvantages just real power.

But why:

-The mixture was absolute stable and safe, safer than the similar M46 formula.The mixture was absolute professional mixture.

-The mixture are more powerful with 3-4 micron aluminum powder than the KClO4+Mg 50/50 mixture what used in M80 salutes.Much more brighter and effective.Its have the KClO4/Mg/S flash powder 50/40/10% (with 400 mesh magnesium powder) all power and extreme sound.Plus its much more stable than a KClO4/Mg 50/50 mixture.

-When you use 20 micron aluminum or blue aluminum in large firecracker have a big effect.The metal powder rich composition some of the metal powder burn in air and not the oxidizer burns it so you will see much better and brighter flash effect.The same technique what used in photoflash powders.

But in flash effect its almost have the Ba(NO3)2 flash powders extreme bright big effect.1,5g in a polumna (triangle) firecracker are 1,5 km far away can hear the extreme powerful sound. And the flash effect in the night are

brightly shiny.

-The ratio was the most strongest KClO4 Al S ratio.Works with coarser aluminum too.The ratio beat all another KClO4/Al/S ratios.

-When you directly ignite it its not faster than other flash powders.But is you put in a paper tube performance can not be compared to other mixtures like:KNO3,KMNO4,Ba(NO3)2,mixtures.

-Its a all in one flash powder: extreme bright,extreme sound,safe,extreme power,plus a professional mixture.

-The KClO4 and sulfur does not attack the aluminum, so you does not need to use boric acid to protect the aluminum.

-Sulfur and aluminum powder are cheap and easy to buy. No extra special costly ingredients are needed what you does not use from something else.

The extreme powerful KClO4 flash powder using a ball mill:The finely powdered 24h in a ball mill milled potassium perchlorate 200°C-300°C heated and cooled down. Than at room temperature mixed with sulfur powder at 5:1 ratio than milled again in a ball mill more 12 hour the 2 component. And mixed 6:4 with 3-4 micron dark aluminum powder, and sifted in a sieve 3-4 times.Thereafter are thoroughly mixed in a mortar and paste in small doses so that the constituents are well mixed and sifted in a sieve again.If the components they are not well-mixed to a homogeneous powder the flash powder will minimum 50% it will be weaker. With KClO4 potassium perchlorate the mixture are stable and highly resistance for friction. And the KClO4+S 5:1 mixture is not flammable. If you carefully mixed together the ingredients mixed in a mortal and pastle to make the ingredients homogeneous.Its will be more than 50% powerful as if the mixtures were just shaken together.Before you use sieve through a sieve so that the powder gets loosened.The mixture are largely resistance for friction so you can safely make it.

But then why is not it so well known like the classic KClO4/Al 70/30 or KClO4/Mg 50:50 mixture?

In professional pyrotechnics one of the goals is cheapness.The other thing is that the mixture is too strong.In homemade pyrotechnics the KClO4 are a costly material.So people use the classic mixtures.Another thing KClO4/Al/S mixtures with more KClO4 or more sulfur you can easy slow down the mixture.Like the Shimizu flash comp 64/23/13. So find the most powerful and best KClO4 flash powder ratio and ingredients need several years of experimentation.

I made a lot of test videos from this composition with various aluminum powders: Homemade from foil, Dark, Dark+Blue, Homemade refined paint grade, 20 micron Al, in a extreme mini and 1Kg firecracker too.

Making flash powder with ball mill: https://www.bitchute.com/video/4YftWQpcrMb3/ or https://odysee.com/@mx5kevin:a/How-To-make-Flash-Powder-with-ball-mill:c

My blog with more description: https://mx5-kevin.blogspot.com or https://sufnipiro.wordpress.com

Videos from this flash powder: https://www.bitchute.com/channel/mx5kevin/

Decentralized pyrotechnic sites on ZeroNet: https://steemit.com/chemistry/@mx5kevin/decentralized-chemistry-and-pyrotechnics-forum-on-zeronet

Sort:  

This flash powder much more better than the classic KClO4/Al 70 30, or KClO4 Mg 50:50. With sulfur the composition are much more brisant, louder and powerful. And the best, fastest, brightest KClO4/Al/S ratio what works coarser aluminum powder too.

Coin Marketplace

STEEM 0.18
TRX 0.16
JST 0.029
BTC 76015.33
ETH 2892.38
USDT 1.00
SBD 2.58